Titanium Alloys
Alloy
Al
V
Sn
Pd/ Fe/ Cr
Mo
Zr
Ni
N max
C max
H max
Fe max
O max
Resid- uals (each) max
Resid- uals (total) max
Ti
ASTM Grade 1
0.03
0.10
0.01
0.20
0.18
0.1
0.40
bal.
ASTM Grade 2
0.30
0.25
ASTM Grade 3
0.05
0.35
ASTM Grade 4
0.50
ASTM Grade 5
5.5- 6.75
3.5-4.5
ASTM Grade 6
4.0- 6.0
2.0-3.0
ASTM Grade 7
Pd 0.12- 0.25
ASTM Grade 9
2.5- 3.5
0.02
0.15
ASTM Grade 11
ASTM Grade 12
0.2-0.4
0.6-0.9
0.08
0.3
Ti 5-2.5 ELI
4.50- 5.75
2.00- 3.00
0.035
0.0125
0.12
Ti 6-4 ELI
5.50- 6.50
0.13
Ti 8-1-1
7.35- 8.35
0.75- 1.25
0.015
Ti 6-6-2
5.00- 6.00
5.0-6.0
1.5-2.5
Fe 0.35- 1.00
0.04
Ti 6-2-4-2
1.8-2.2
3.6- 4.4
Ti 6-2-4-6
1.75- 2.25
5.5-6.5
Ti 7-4
6.50- 7.30
0.013
Ti 8-8-2-3
2.60- 3.40
7.5-8.5
Fe 1.60- 2.40
0.16
Ti 15-3-3-3
14.0- 16.0
Cr 2.5- 3.5
Ti 13-11-3
2.50- 3.50
12.5- 14.5
Cr 10.0- 12.0
0.025
0.17
b