Nickel Base Alloys

  Ni Cr Co Mo W Fe Al Ti Cu Nb Others
Hastelloy A

57

1.0*

-

21

-

19

-

-

-

-

-

Hastelloy B

62

1.0*

2.5*

28

-

5.5

-

-

-

-

0.4 V

Hastelloy B2

66

1.0*

0.75*

28

-

2.0*

0.4*

-

-

-

-

Hastelloy C276

56

16

2.5*

17

4

5.5

0.4*

-

-

-

0.35* V

Hastelloy C22

54

21

2.5*

14

3

5.0*

0.4*

-

-

-

0.35* V

Hastelloy C4

54

16

1.25*

16

-

2.0*

0.4*

0.5*

-

-

-

Hastelloy D

85

1.0*

-

-

-

1.0*

-

-

4.0*

-

9 Si

Hastelloy F

45

22

2.5*

6

1.0*

18

-

-

-

2

-

Hastelloy G

44

22

-

6.5

1.0*

20

-

-

2

2

-

Hastelloy N

72

7

0.2

16.5

0.5

5.0*

0.25

0.25

-

-

0.01 B

Hastelloy R

66

15.5

1.5*

5

-

7.0*

2.2

2.5

-

-

-

Hastelloy S

68

15.5

-

14.5

-

1

-

-

-

-

0.5 Mn
0.4 Si

Hastelloy W

63

5

2.5*

24.5

-

5.5

-

-

-

-

0.6 V

Hastelloy X

47

22

1.5

9

0.6

18.5

-

-

-

-

-

Inconel 600

75.5

15.5

-

-

-

7

-

-

-

-

-

Inconel 601

60.5

23

-

-

-

14.1

1.35

-

-

-

-

Inconel 625

61

21.5

-

9

-

3

-

-

-

3

-

Inconel 690

61

29

-

-

-

9

-

-

-

-

-

Inconel 702

79

15.6

-

-

-

0.4

3.4

0.7

-

-

-

Inconel 706

41.5

16

1

-

-

36

-

1.75

-

2.9

-

Inconel 713C

72

13.4

-

4.5

-

1.5*

6.2

1.0*

-

2.3

-

Inconel 718

53

18.5

-

3

-

18

-

0.8

-

5

-

Inconel W(722)

75

15

-

-

-

6.5

0.6

2.4

-

-

-

Inconel X(X750)

73

15

1

-

-

7

0.9

2.5

-

0.9

-

RENE 80

60.5

13.5

9.5

4

4

-

3

5

-

-

0.015B 0.04Zr 

IN-657

49

48

-

-

-

-

-

-

-

1.5

-

Incoloy 800

32

20

-

-

-

47

-

-

-

-

-

Incoloy 825

40

21

-

3

-

32

-

1

2

-

-

Incoloy 901

42

12.5

1.0*

5.7

-

35

0.35*

2.9

-

-

-

AISI 310(HK)

20

25

-

-

-

BAL

-

-

-

-

2 Mn
2 Si
0.35 C

AISI 330(HT)

35

15

-

-

-

BAL

-

-

-

-

2.5 Si

Nimonic 75

77

20

-

-

-

5.0*

0.15

0.4

-

-

-

Nimonic 80

74

20

2.0*

-

-

1.5*

1.3

2.2

-

-

-

Nimonic 81

65

30

-

-

-

1.0*

1

1.75

-

-

-

Nimonic 86

64.5

25

-

10

-

-

-

-

-

-

0.15 Mn
0.03 Ce

Nimonic 942

48

12.5

1.0*

5.5

-

25

4

3.7

-

-

0.015 B

* indicates maximum